Measurement of temperatures and heat effects of phase transition; measurement of specific heat capacity of substances and materials; investigation of compatibility of crystal substances; investigation of oxidative stability of substances and materials.
technical characteristics:
Temperature range from -180 to 700°C;
Controlled heating rates and cooling rates from 0.1 to 100 ̊C/min;